Friction Stir Welding of AZ31B-H24 Magnesium Alloy in Lap Configuration
Notice bibliographique
Résumé
Friction stir welding (FSW) being an enabling solid-state joining technology can be suitably applied for the assembly of lightweight magnesium alloys. In this study, AZ31B-H24 Mg alloy sheets with a thickness of 2 mm were friction stir welded in lap configuration using two tool rotational rates of 1000 and 1500 rpm and two welding speeds of 10 and 20 mm/s. The joint quality was characterized in terms of the residual stresses, welding defects, microstructure, and texture. The mechanical properties including hardness, room and elevated temperature tensile and fatigue properties were also evaluated and correlated to the structure and defects. It was observed that the hardness decreased from the base metal (BM) to the stir zone (SZ) across the heat-affected zone (HAZ) and thermomechanically-affected zone (TMAZ). The lowest value of hardness appeared in the SZ. With increasing tool rotational rate or decreasing welding speed, the average hardness in the SZ decreased owing to increasing grain sizes, and a Hall-Petch-type relationship was established. The shear tensile behavior of the lap joints was evaluated at low (-40°C), room (25°C), and elevated (180°C) temperatures. The failure load was highest in the lower heat input condition that was obtained at a tool rotational rate of 1000 rpm and a welding speed of 20 mm/s at all the test temperatures, due to a smaller hooking height, larger effective sheet thickness, and lower tensile residual stress, as compared with other two welding conditions that were obtained at a higher tool rotational rate or lower welding speed. The lap joints usually fractured on the advancing side of the top sheet near the interface between the TMAZ and the SZ. Elevated temperature testing of the weld assembled at a tool rotational rate of 1000 rpm and a welding speed of 20 mm/s led to the failure along the sheet interface in a shear fracture mode due to the high integrity of the joint that exhibited large plastic deformation and increased total energy absorption. Fatigue fracture of the lap welds always occurred at the interface between the SZ and TMAZ on the advancing side where a larger hooking defect was present (in comparison with the retreating side). The welding parameters had a significant influence on the hook height and the subsequent fatigue life. A relatively “cold” weld, conducted at a rotational rate of 1000 rpm and welding speed of 20 mm/s, gave rise to almost complete elimination of the hooking defect, thus considerably (over two orders of magnitude) improving the fatigue life. Fatigue crack propagation was basically characterized by the formation of fatigue striations concomitantly with secondary cracks.
Récupéré en direct depuis OpenAlex et désinversé. Les résumés ne sont pas conservés dans cette base de données : les index inversés représentent 8,6 Go des 9,3 Go de texte de la base, et le serveur dispose de 13 Go libres.
Comment cette classification a été obtenuedéplier
Prédiction distillée sur la base complète
Imitation des enseignantsNi prévalence calibrée, ni vérité terrain. Validation humaine à venir. Apprise à partir de 10 348 étiquettes directes de Codex et de 10 348 étiquettes directes de Gemma. Le mode candidate est l'union des têtes enseignantes seuillées; le consensus est leur intersection. Ces sorties portent le statut machine_predicted_unvalidated et ne sont ni des étiquettes humaines ni des étiquettes directes de modèles de pointe.
Scores Codex et Gemma par catégorie
| Catégorie | Codex | Gemma |
|---|---|---|
| Métarecherche | 0,000 | 0,000 |
| Méta-épidémiologie (sens strict) | 0,000 | 0,000 |
| Méta-épidémiologie (sens large) | 0,000 | 0,000 |
| Bibliométrie | 0,000 | 0,000 |
| Études des sciences et des technologies | 0,000 | 0,000 |
| Communication savante | 0,000 | 0,000 |
| Science ouverte | 0,000 | 0,000 |
| Intégrité de la recherche | 0,000 | 0,000 |
| Charge utile insuffisante (le modèle a refusé de juger) | 0,000 | 0,000 |
Scores machine (provisoires)
Les deux têtes enseignantes du modèle étudiant, lues sur ce travail. Un score ordonne la base pour la relecture; il n'affirme jamais une catégorie, et le statut de validation accompagne chaque rangée tel quel.
Scores de référence d'un modèle non mature (critères de maturité non atteints, 7 itérations). Un score ordonne; il n'affirme jamais une catégorie.
score_only:v0-immature-baseline · tel quel depuis la passe de notation : score_only signifie que le nombre peut ordonner les travaux, et qu'aucune étiquette de catégorie n'en découleClassification
machine, non validéePrédiction automatique; un appel candidat d’une seule tête enseignante, pas un consensus.
Le détail, modèle par modèle et score par score, se trouve en fin de page sous « Comment cette classification a été obtenue ».