Hydrogen embrittlement characteristics of two tempered martensitic steel alloys for high-strength bolting
Notice bibliographique
Résumé
Hydrogen embrittlement threshold curves were derived for two quenched and tempered steel grades, AISI 4135 and AISI 4340, at varying hardness ranging from 33 to 54 HRC. For each material, hydrogen was introduced (i) by zinc electroplating as a worst case condition for internal hydrogen embrittlement and (ii) by imposing cathodic potential of −1.2 V as a worst case condition for environmental hydrogen embrittlement. Overall, AISI 4135 exhibited lower thresholds than AISI 4340, making it the more susceptible of the two alloys. The findings demonstrate although hardness and/or strength have a first-order effect on hydrogen embrittlement susceptibility, difference in chemistry leading to differences microstructural characteristics must also be considered. Below hardness of 39 HRC, both alloys were not susceptible to internal hydrogen embrittlement, a finding that is consistent with common industry practice and fastener electroplating standards that do not mandate baking of electroplated fasteners with specified hardness below 39 HRC.
Récupéré en direct depuis OpenAlex et désinversé. Les résumés ne sont pas conservés dans cette base de données : les index inversés représentent 8,6 Go des 9,3 Go de texte de la base, et le serveur dispose de 13 Go libres.
Comment cette classification a été obtenuedéplier
Prédiction machine sur la base complète
Imitation des enseignantsNi prévalence calibrée, ni vérité terrain. Validation humaine à venir. Le volet Gemma est une étiquette directe du modèle pour chaque travail de la base, lue sur la notice réduite au titre. Le volet Codex est un classifieur appris des 10 348 étiquettes directes de Codex et calibré sur les taux pondérés de l'échantillon; les champs sans appui suffisant ne portent aucun appel Codex. Le mode candidate est l'union des deux volets; le consensus est leur intersection. Ces sorties portent le statut machine_predicted_unvalidated et ne sont pas des étiquettes humaines.
Scores du classifieur distillé par catégorie (deux têtes)
| Catégorie | Codex | Gemma |
|---|---|---|
| Métarecherche | 0,000 | 0,001 |
| Méta-épidémiologie (sens strict) | 0,000 | 0,000 |
| Méta-épidémiologie (sens large) | 0,000 | 0,000 |
| Bibliométrie | 0,001 | 0,000 |
| Études des sciences et des technologies | 0,000 | 0,000 |
| Communication savante | 0,000 | 0,000 |
| Science ouverte | 0,000 | 0,000 |
| Intégrité de la recherche | 0,000 | 0,000 |
| Charge utile insuffisante (le modèle a refusé de juger) | 0,001 | 0,000 |
Scores machine (provisoires)
Les deux têtes enseignantes du modèle étudiant, lues sur ce travail. Un score ordonne la base pour la relecture; il n'affirme jamais une catégorie, et le statut de validation accompagne chaque rangée tel quel.
Scores de référence d'un modèle non mature (critères de maturité non atteints, 7 itérations). Un score ordonne; il n'affirme jamais une catégorie.
score_only:v0-immature-baseline · tel quel depuis la passe de notation : score_only signifie que le nombre peut ordonner les travaux, et qu'aucune étiquette de catégorie n'en découleClassification
machine, non validéePrédiction automatique; un appel candidat d’une seule source (Gemma direct ou Codex distillé), pas un consensus.
Le détail, modèle par modèle et score par score, se trouve en fin de page sous « Comment cette classification a été obtenue ».